,cnc machinist,cnc manufacturing,cnc mechanic,cnc mill,cnc milling center,cnc milling companies,cnc milling tools,cnc parts,cnc plasma cutter,cnc plasma cutting,cnc plasma table,cnc production,cnc router table,cnc screw machine,cnc service,cnc swiss,cnc turning,cnc turning center,cnc turning centers,cnc vertical lathe,horizontal cnc,how to cnc machine,machining cnc,manufacturing cnc machines,okuma cnc,plasma cnc machine,production cnc machining,troubleshooting cnc machines,used cnc machine tools,used cnc milling machines,vertical cnc lathe,what can a cnc machine make
1.yearly output from 30000-120000M3.2.on site installation
3.professional manufacturer since 1990!
Full automatic particle board line
1) Chip preparation section
Wood, branches and wood residues are cut into chips of definite size. Chips from chips silo will be screened or airgradeed to remove fines,soil and stones.
2) Fiber preparation section
Chips are transported to upper bin of refiner, and positively fed to digester by screw feeder for steaming. Steam chips will be distintegrated to fiber under the force of heat and mechanism. Mix drying medium and wet fiber which is in the state of suspension with the help of high pressure air flow,and thus exhaust moisure in fiber via drying medium to ger dry fiber. Dry fiber falls on belt conveyor through cylone discharge valve, and then be transported to dry fiber bin for storage.
3) Glue mixing and applying section
Process of glue applying before drying is adotpted.Feed molten paraffin and water-proof additive to fefiner. Paraffin is mixed with fiber uniformly under the force of refiner plates. Glue is transported to the below line of fiber discharge valve. With the help of 28-30m/s high speed air-flow,glue mist meets and attachs to the surface of fiber. This section can be controlled by PLC or computer.
4) Mat-forming and hot-pressing section
The fiber after drying is transported to the above of forming machine, and uniformly spread on the conveying mesh belt in the way of air-flow.Vacuum box equipped below the mesh belt provides negative pressure and air will be removed via mesh belt,fiber stays on mesh belt and thereafter forms mats gradually. Fluffy mats will be pressed by pre-press. Pressed mats are cut into definite length by longitudinal and transversal saw, then transproted to loader passing through accelerating conveyor, stoage conveyor and extension conveyor. When finishing loading mats,carriage in the loader will feed conveying belt and mats into hot press,at the same time, shovel head at the front end of conveying belt pushes out pressed board.When carriage coms to terminal,boards have been into unloader,and mats also arrives to due position.Carriage returns,conveying belt turns forward. Mats are in relative still state and stay on the platen of press when velocity of conveying belt is the same as the returning speed of carriage. Glue in the mats cures ,thanks to temperature and pressure in hot press, and hence boards with definite intensity and thickness form. Rough boards will be put on support via loader. Outfeeding conveyor will unload boards one after another to next section when cage comes down.
5) Cooling, sizing and sanding section
Rough boards after air cooling are turned in to cut-to-size boards via longitudinal and transversal saw. And then cut-to-size boards are sanded, sorted, stacked and packed for sorage.